Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Malvern Minerals Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product data demonstrates the effect of the Novakup (lamellar quartz surface treated with 0.5% A-1100) filler. A separate entry demonstrates the effect of untreated Novacite filler in thermoplastic polyester. The specific thermoplastic polyester is J-105.Information provided by Malvern Minerals Company.
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.1 MPa
6100 psi
after 16 hours in 50°C water
46.9 MPa
6800 psi
initial
Flexural Strength 95.8 MPa
13900 psi
after 16 hours in 50°C water
98.6 MPa
14300 psi
initial
Flexural Modulus 5.58 GPa
810 ksi
initial
5.58 GPa
810 ksi
after 16 hours in 50°C water
Izod Impact, Unnotched 1.39 J/cm
2.60 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F