Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.58 GPa | 810 ksi | initial |
Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler Product data demonstrates the effect of the Novakup (lamellar quartz surface treated with 0.5% A-1100) filler. A separate entry demonstrates the effect of untreated Novacite filler in thermopla.. |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | after 16 hours in 50°C water |
Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler Product data demonstrates the effect of the Novakup (lamellar quartz surface treated with 0.5% A-1100) filler. A separate entry demonstrates the effect of untreated Novacite filler in thermopla.. |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 WM40 IM HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessin.. |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | ASTM D790 |
Clariant Renol 6004G23 Nylon 6, 23% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | |
BCC Products BC 7009-2 Epoxy Casting BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in m.. |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | ASTM D790 |
PlastxWorld CEVIAN® SUG20 ABS Glass fiber reinforced, high heat resistant and flame retarded ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by P.. |