Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.58 GPa | 810 ksi | initial |
Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler Product data demonstrates the effect of the Novakup (lamellar quartz surface treated with 0.5% A-1100) filler. A separate entry demonstrates the effect of untreated Novacite filler in thermopla.. |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | after 16 hours in 50°C water |
Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler Product data demonstrates the effect of the Novakup (lamellar quartz surface treated with 0.5% A-1100) filler. A separate entry demonstrates the effect of untreated Novacite filler in thermopla.. |
|||
Flexural Modulus | 5.58 GPa | 809 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL S100G20 PPE+PS (Asia Pacific) |
|||
Flexural Modulus | 5.58 GPa | 809 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2312EPR PEI 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Flexural Modulus | 5.58 GPa | 809 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Flexural Modulus | 5.58 GPa | 809 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Flexural Modulus | 5.58 GPa | 809 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM CRS5711 PEI 15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 5.58 GPa | 809 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM CRS5711 PEI (Asia Pacific) 15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 5.58 GPa | 809 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MX01739C PP LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Modulus | 5.58 GPa | 809 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC LNP THERMOCOMP* DF004ER is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. Mold Release. |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 WM40 IM HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessin.. |
|||
Flexural Modulus | 5.58 GPa | 809 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RX06420 PA 66 LNP* Thermocomp* RX06420 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Low Extractible, Mold Release. |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | ASTM D790 |
Clariant Renol 6004G23 Nylon 6, 23% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | |
BCC Products BC 7009-2 Epoxy Casting BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in m.. |
|||
Flexural Modulus | 5.58 GPa | 810 ksi | ASTM D790 |
PlastxWorld CEVIAN® SUG20 ABS Glass fiber reinforced, high heat resistant and flame retarded ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by P.. |