Mechanical Properties Metric English Comments
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Niche Polymer PCM18BK PC
Information provided by Niche Polymer
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow
Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release
Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow
Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release
Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow
Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow
Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release
Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release
Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release
Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow
Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow
Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Polymer Resources PC-UV3-D-[color]-1 Polycarbonate, UV-stabilized, High Flow with Mold Release
Polycarbonate, UV-stabilized, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Flexural Strength 95.8 MPa
13900 psi
after 16 hours in 50°C water
Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler
Product data demonstrates the effect of the Novakup (lamellar quartz surface treated with 0.5% A-1100) filler. A separate entry demonstrates the effect of untreated Novacite filler in thermopla..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Techmer ES Statiblend® POM CO
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeature: ConductiveTPCI# 9962114Information provided by TP Composites, Inc.
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Chase Plastics CP Pryme® NN113GL (COND, 50% RH) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Entec Hylex® P1017L1 HB Polycarbonate
Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Clear/Transparent Information provided by Entec
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Entec Hylex® P1017L2 HB Polycarbonate
Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Blue Information provided by Entec
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Entec Hylex® P1317L1 HB Polycarbonate
UV Stabilized, Higher Flow, Mold Release, Water ClearInformation provided by Entec.
Flexural Strength 95.8 MPa

@Temperature 150 °C
13900 psi

@Temperature 302 °F
ISO 178
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Techmer ES HiFill FR® PBT 0166 B FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.