Material Notes:
Description: SEQUEL® 1480 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paintability, and processability. SEQUEL® 1480 offers improved scratch and mar resistance compared to typical TPO products. Applications: Bumper fascias, body side molding, sills Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ISO 1183
Linear Mold Shrinkage 0.0080 - 0.011 cm/cm
0.0080 - 0.011 in/in
as molded; ISO 294
0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
after bake; ISO 294
Melt Flow 29 g/10 min
29 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.6 MPa
2700 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.336 GPa
193.8 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 18.0 J
13.3 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 75.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
41.7 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228