LyondellBasell Lupolen® V 2920 K Ethylene Vinyl Acetate, lnjection Molding Grade

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer LyondellBasell
Trade Name Lupolen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Lupolen® V 2920 K Ethylene Vinyl Acetate, lnjection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.00 MPa
1160 psi
Elongation at Break >= 50 %
>= 50 %
Tensile Modulus 0.105 GPa
15.2 ksi
Thermal Properties Metric English Comments
Melting Point 97.0 °C
207 °F
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
Dissipation Factor 0.013

@Frequency 100 Hz
0.013

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V