Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 97.0 °C | 207 °F | Internal Method |
Polimeri Europa Greenflex® ML 30 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion Greenflex ML 30 is an ethylene vinyl acetate copolymer (EVA) for injection molding and profile extrusion. Items produced with Greenflex ML 30 show good ESCR and elasticity.Main Applications: Green.. |
|||
Melting Point | 97.0 °C | 207 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Melting Point | 97.0 °C | 207 °F | |
LyondellBasell Lupolen® V 2920 K Ethylene Vinyl Acetate, lnjection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 97.0 °C | 207 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Melting Point | 97.0 °C | 207 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating 9 wt% Acrylic Acid.Nucrel® 3990 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to .. |
|||
Melting Point | 97.0 °C | 207 °F | ISO 11357 |
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi.. |
|||
Melting Point | 97.0 °C | 207 °F | Peak; ASTM D3418 |
Westlake EMAC® EF598AA 9% Ethylene-Methyl Acrylate Copolymer Clarity optics, excellent drawdown, excellent machinability, good TD heat shrinkage and excellent toughness. Uses include food packaging tie layers, heat seal layers, extrusion coating, cast film, .. |
|||
Melting Point | 97.0 °C | 207 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers exce.. |
|||
Melting Point | 97.2 °C | 207 °F | Peak Melting Temperature; ISO 11357-3 |
ExxonMobil EXACT™ 0210 Ethylene-based Plastomer for Multilayer Film Applications Exact 0210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications requiring good flow/caul.. |
|||
Melting Point | 97.2 °C | 207 °F | DSC peak melting point; ASTM D3418 |
ExxonMobil EXACT™ 0230 Plastomer for Multilayer Film Applications Product Description: Exact 0230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for both monolayer and multilayer co-extruded cast .. |
|||
Melting Point | 97.2 °C | 207 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil EXACT™ 3024 Plastomer for Cast Film Applications Product Description: Exact 3024 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It can be used for both monolayer and multilayer coextruded .. |
|||
Melting Point | 97.0 °C | 207 °F | ASTM D3418, ISO 3146 |
DuPont™ Appeel® 20D828 Ethylene Acrylate Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp.. |
|||
Melting Point | 97.0 °C | 207 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Melting Point | 97.0 °C | 207 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Melting Point | 97.0 °C | 207 °F | Freezing Point; ASTM D3418 |
DuPont™ Fusabond® E528 Polymer Modifier DuPont™ Fusabond® E528 is a anhydride modified polyethylene. Used as a polymer modifier |
|||
Melting Point | 97.0 °C | 207 °F | ASTM D3418, ISO 3146 |
DuPont™ Nucrel® 3990L Ethylene Acrylic Acid Nucrel® 3990L is a copolymer of ethylene and acrylic acid. It is available for use in conventional extrusion coating, coextrusion coating and extrusion laminating equipment. 9.5 % By Weight Acrylic.. |
|||
Melting Point | 97.0 °C | 207 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Melting Point | 97.0 °C | 207 °F | ASTM D3417, ISO 3146 |
DuPont™ Surlyn® 1825 Zinc Ionomer Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp.. |
|||
Melting Point | 97.0 °C | 207 °F | ASTM D3417, ISO 3146 |
DuPont™ Surlyn® 2601B Sodium Ionomer Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer .. |
|||
Melting Point | 97.0 °C | 207 °F | Exxon Method |
ExxonMobil Escorene® LD-712 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness... |
|||
Melting Point | 97.2 °C | 207 °F | |
M. Holland Company MAGMA® LM124-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melting Point | 97.2 °C | 207 °F | ASTM D3218 |
M. Holland Company MAGMA® LM233-A LLDPE
(discontinued **) Features: Good Heat Seal, Good ProcessabilityUses: Coating Applications, Film, Cast Film, PackagingProcessing Method: Coextrusion, Blown FilmInformation provided by M. Holland. |
|||
Melting Point | 97.0 °C | 207 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinued 12 wt% Methacrylic Acid.Nucrel® 1214 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des.. |