CMT Materials HYTAC® B Solid Polymer Tooling Material

Category Polymer , Thermoplastic
Manufacturer CMT Materials
Trade Name HYTAC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials HYTAC® B Solid Polymer Tooling Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sometimes, finer plug assist details are required which are not obtainable or maintainable with syntactic foam plugs. For these high detail applications, where high toughness and easy machinability are required, we have formulated a special blend of engineering thermoplastic polymer. Material removal from the blind side of the plug will result in thermal conductivity and overall heat absorption which approximate syntactic foam's excellent properties. High Toughness and Durability: With high toughness, machine downtime due to damage plugs is reduced. Less downtime = lower costs = more consistent quality. Good Machinability: No dust collection equipment or respirators are required due to the large, non-abrasive chips. Plugs can be machined over 3x faster than syntactic foam due to the easy chip formation. Excellent Temperature Resistance: HYTAC-B is specially formulated for service temperatures up to 350°F with minimal loss in mechanical properties. Variety of Shapes and Sizes: The material is provided in standard sized sheets. Applications: HYTAC-B is primarily used as a heat resistant replacement for nylon. Typically used in shallow draw applications where material distribution is not critical. Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 1.12 - 1.19 g/cc
0.0405 - 0.0428 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 82.7 MPa
12000 psi
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.360 W/m-K
2.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
Descriptive Properties Value Comments
Color Blue