Material Notes:
Silvaloy 18M is a ternary alloy of silver, phosphorus, and copper approaching the eutectic composition. It is very fluid at brazing temperature and should be used on well fitted joints. Silvaloy 18M low brazing temperature and narrow solidus, liquidus range makes it ideal for applications where temperature is a factor with slow heating rates, such as in furnace brazing.Applications:Silvaloy 18M is used for joining copper and copper alloys, such as brass or bronze. It is suitable for use on silver, tungsten, and molybdenum. It should not be used on ferrous nickel alloys. On copper to copper applications, it is self-fluxing due to the fluxing action of the phosphorus content. It's low melting temperature makes it ideal for application on copper to brass temperature and dezincification is a factor.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 8.35 g/cc
8.35 g/cc
Density 8.36 g/cc
0.302 lb/in³
Thermal Properties Metric English Comments
Melting Point 643 - 668.3 °C
1190 - 1235 °F
Solidus 643 °C
1190 °F
Liquidus 668.3 °C
1235 °F
Maximum Service Temperature, Air 204 °C
400 °F
continuous
260 °C
500 °F
intermittent
Component Elements Properties Metric English Comments
Copper, Cu 74.35 - 77 %
74.35 - 77 %
As balance
Other, total <= 0.15 %
<= 0.15 %
Phosphorous, P 6.0 - 6.5 %
6.0 - 6.5 %
Silver, Ag 17 - 19 %
17 - 19 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000290 ohm-cm
0.0000290 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 662.8 - 732 °C
1225 - 1350 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Copper
Electrical Conductivity (% IACS) 6