Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 8.35 g/cc | 8.35 g/cc | |
Lucas-Milhaupt Silvaloy® X55 Brazing Alloy Silvaloy X55 has excellent gap filling capability and plasticity when in the molten condition. It also exhibits excellent strength and ductility while cooling from the liquid stage. The improved str.. |
|||
Specific Gravity | 8.35 g/cc | 8.35 g/cc | |
Lucas-Milhaupt Silvaloy® 18M Brazing Alloy Silvaloy 18M is a ternary alloy of silver, phosphorus, and copper approaching the eutectic composition. It is very fluid at brazing temperature and should be used on well fitted joints. Silvaloy 18M.. |