Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 618.3 - 732 °C | 1145 - 1350 °F | Brazing Range |
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet.. |
|||
Processing Temperature | 662.8 - 732 °C | 1225 - 1350 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 18M Brazing Alloy Silvaloy 18M is a ternary alloy of silver, phosphorus, and copper approaching the eutectic composition. It is very fluid at brazing temperature and should be used on well fitted joints. Silvaloy 18M.. |