Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 643 °C | 1190 °F | |
Johnson Matthey Matti-sil 453S Cadmium Free Brazing Alloy The 45% Silver alloys, with tin and silicon, are more free flowing than Matti-sil 45 and less costly than Matti-sil 56Sn.Optimum Joint Gap 0.05 - 0.15 mm.Federal Specification QQ-B-564 BAg-8aInforma.. |
|||
Solidus | 643 °C | 1190 °F | Melting Point |
Lucas-Milhaupt SIL-FOS 18 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 18 is a moderate cost brazing filler metal suitable for joining copper, brass and bronze alloys where low brazing temperature and free flowing characteristics are required. I.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvabraze 33830 Brazing Alloy Silvabraze is used for brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten, and molybdenum. It is primarily used for the joining of copper-to-copper on vib.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvalite Brazing Alloy SILVALITE is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on v.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 2M Brazing Alloy Silvaloy 2M is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 18M Brazing Alloy Silvaloy 18M is a ternary alloy of silver, phosphorus, and copper approaching the eutectic composition. It is very fluid at brazing temperature and should be used on well fitted joints. Silvaloy 18M.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 2 Brazing Alloy Silvaloy 2 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 5 Brazing Alloy Silvaloy 5 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 6 Brazing Alloy Silvaloy 6 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It should not be used on ferrous and nickel metals or copper.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 15 Brazing Alloy Silvaloy 15 is used for the brazing of copper and copper alloys, brass, and bronze. It can also be used on silver, tungsten and molybdenum. It is very effective for joining pipe and tubing and is wi.. |