Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000290 ohm-cm | 0.0000290 ohm-cm | |
Indium Corp. Indalloy® 233 Pb-Sb-Sn Solder Alloy Intermediate temp solder. Creep resistant.Information provided by the manufacturer, Indium Corporation. |
|||
Electrical Resistivity | 0.0000290 ohm-cm | 0.0000290 ohm-cm | |
Indium Corp. Indalloy® 7 In-Pb Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Electrical Resistivity | 0.0000290 ohm-cm | 0.0000290 ohm-cm | |
Indium Corp. Indalloy 229 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Electrical Resistivity | 0.0000290 ohm-cm | 0.0000290 ohm-cm | |
Indium Corp. Indalloy® 165 Pb-Ag-Sn Solder Alloy Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly. Often used in reducing atmospheres such as 12% hydrogen. Slightly better corrosion resistance than #101.Inf.. |
|||
Electrical Resistivity | 0.0000290 ohm-cm | 0.0000290 ohm-cm | |
Lucas-Milhaupt Silvaloy® 18M Brazing Alloy Silvaloy 18M is a ternary alloy of silver, phosphorus, and copper approaching the eutectic composition. It is very fluid at brazing temperature and should be used on well fitted joints. Silvaloy 18M.. |
|||
Electrical Resistivity | 0.0000290 ohm-cm | 0.0000290 ohm-cm | Temperature Coefficient of 0.0003/K |
Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver Good machinability, excellent cold working and welding characteristics. Poor hot forming. Uses include rivets, screws, zippers, optical parts and costume jewelry.Information provided by Goodfello.. |
|||
Electrical Resistivity | 0.0000290 - 0.0000330 ohm-cm | 0.0000290 - 0.0000330 ohm-cm | Temperature Coefficient of 0.0019/K |
Goodfellow T2-Thermocouple Alloy The negative element of the type K thermocouple, the positive being T1. The thermocouple can be used up to 1250C in oxidizing atmospheres, and probably is the most common in use.Information provided.. |
|||
Electrical Resistivity | 0.0000290 ohm-cm | 0.0000290 ohm-cm | |
Goodfellow Tungsten 75/Rhenium 25 Alloy When used with Tungsten the alloy is an important high temperature thermocouple wire. The alloy can also be used as a filament.Information provided by Goodfellow. |