Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 662.8 - 732 °C | 1225 - 1350 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 18M Brazing Alloy Silvaloy 18M is a ternary alloy of silver, phosphorus, and copper approaching the eutectic composition. It is very fluid at brazing temperature and should be used on well fitted joints. Silvaloy 18M.. |