Lubrizol Stat-Rite® S-680 Static Control PETG Alloy

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , PETG Copolyester
Manufacturer Lubrizol (former Noveon)
Trade Name Stat-Rite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Stat-Rite® S-680 Static Control PETG Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components. Features:Permanent static dissipative performanceHumidity insensitiveUltra-clean: low off-gassing, low ionic contaminationColorableDurable: Can be used repeatedly.Applications:Hard disk packagingMedical device packagingElectronic component handlingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Tensile Modulus 1.10 GPa
160 ksi
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790-92
Izod Impact, Notched 9.61 J/cm
18.0 ft-lb/in
ASTM D256-92
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+9 ohm-cm
2.00e+9 ohm-cm
50% RH; ASTM D257
Surface Resistance 8.00e+8 ohm
8.00e+8 ohm
ESD S11.11; 12 % R.H.
Surface Resistivity per Square 2.00e+9 ohm
2.00e+9 ohm
ASTM D257
Static Decay 0.010 sec
0.010 sec
FTMS-101C; 12% R.H., (+5000 V to 50 V)
0.010 sec
0.010 sec
FTMS-101C; 12% R.H., (-5000 V to -50 V)
0.10 sec
0.10 sec
Charged Plate Monitor; 50% R.H. MD, (+1000 V to 10 V)
Tribocharge 10 V
10 V
Nitrile Glove - BFG Test Method
Descriptive Properties Value Comments
Color Light Blue