Electrical Properties Metric English Comments
Surface Resistivity per Square 2.00e+9 ohm
2.00e+9 ohm
ASTM D257
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy
Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio..
Surface Resistivity per Square 2.00e+9 ohm
2.00e+9 ohm
50% RH; ASTM D257
Lubrizol Stat-Rite® SIS535 Static Control System
Product Description: Stat-Rite® SIS535 is a static dissipative HIPS alloy. Stat-Rite SIS535 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, perma..