Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0160 GPa | 2.32 ksi | ISO 37 |
Huntsman AVALON® 90 AB Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
300% Modulus | 0.0160 GPa | 2.32 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
300% Modulus | 0.0160 GPa | 2.32 ksi | Vulcanized |
KKPC KOSYN 1500S Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
300% Modulus | 0.0160 GPa | 2.32 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
300% Modulus | 0.0160 GPa | 2.32 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer Type: Pearlthane® D91F88 is an aliphatic-based thermoplastic polyurethane.Main Application : ExtrusionSpecial features : Outstanding abrasion loss, excellent color stability upon weather exposure.. |
|||
300% Modulus | 0.0160 GPa | 2.32 ksi | ISO 37 |
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
300% Modulus | 0.0160 GPa | 2.32 ksi | ISO 37 |
Huntsman AVALON® 90 AK Thermoplastic Polyurethane Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har.. |
|||
300% Modulus | 0.0160 GPa | 2.32 ksi | ISO 37 |
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha.. |
|||
300% Modulus | 0.0160 GPa | 2.32 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 92 E 4670 TPU-Polyester Introduction IROGRAN A 92 E 4670 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe.. |
|||
300% Modulus | 0.0160 GPa | 2.32 ksi | Injection molded parts; DIN 53504 |