Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0110 GPa | 1.60 ksi | |
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AR elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced mold release, low compression set, a.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester Introduction: IROGRAN A 94 E 4900 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ISO 37 |
Huntsman AVALON® 95 AE Thermoplastic Polyurethane Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ISO 37 |
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D412 |
SK Chemicals SKYTHANE® R195A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-A895 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | DIN 53504 |
Lubrizol ESTANE® 5707F1 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D412 |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D412 |
Lubrizol Estane® ALR E95A Thermoplastic Polyurethane Type: Estane® ALR E95A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | DIN 53504 |
Lubrizol ESTANE® 5722 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D638 |
ELASTO UK Dryflex® 422451S SBS Based Material, 45D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | JIS-A-5756 |
Denka VINYKON W1051 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® SMR1450 Thermoplastic Polyolefin Elastomer Elastocon® SMR1450 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D638 |
Colorite Polymers 8300 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D638 |
Colorite Polymers 8302 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D638 |
Colorite Polymers 8334 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D638 |
Colorite Polymers 8577 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 9149 Wire & Cable Flexible PVC Highly flame retardant FT-4 tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 9149A Wire & Cable Flexible PVC Highly flame retardant tray cable (FT-4) jacket for 105C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 17890 Wire & Cable Flexible PVC Non-lead stabilized insulation compound recommended for THW and 90C Class 43 applications. UL recognized component for THW and TW.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 18901 Wire & Cable Flexible PVC General purpose, non-lead stabilized, 105°C rated jacketing compound. Formulated to have good migration resistance and flame retardant properties.Information provided by Georgia GulfGeorgia Gulf b.. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 8850 Moldings & Extrusions Flexible PVC General purpose extrusion.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 8862 Moldings & Extrusions Flexible PVC General purpose, clear extrusion compound suitable for speaker wire applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 8862 Wire & Cable Flexible PVC A clear, stain resistant, general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 8881 Moldings & Extrusions Flexible PVC Profile extrusion compound especially formulated to impart a matte surface appearance to the finished article.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 8906 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for applications requiring microbial resistance and good toughness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 18860 Wire & Cable Flexible PVC Flame retardant jacketing compound recommended for a maximum service temperature rating of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D-638 |
Axiall 2258 Wire & Cable Flexible PVC TW insulation suitable for 105°C AWM applications. UL recognized for TW, Oil resistant I and VW-1.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0110 GPa | 1.60 ksi | Original |
DuPont Vamac® DHC Ethylene Acrylic Elastomer
(discontinued **) DuPont™ Vamac® DHC is a dipolymer of ethylene and methylacrylate cured using peroxide vulcanization systems. This gum elastomer includes a small amount of processing aid. It has a mild acrylic odo.. |