Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® 11T60D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent mechanical properties.All information provided by Merquinsa
Physical Properties Metric English Comments
Density 1.19 g/cc

@Temperature 20.0 °C
0.0430 lb/in³

@Temperature 68.0 °F
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ISO 868
Tensile Strength, Yield 40.00 MPa
5801 psi
ISO 527-2/5A/500
Elongation at Break 480 %
480 %
Ultimate; ISO 527-2/5A/500
50% Modulus 0.0150 GPa
2.18 ksi
ISO 527-2/5A/500
100% Modulus 0.01501 GPa
2.177 ksi
ISO 527-2/5A/500
300% Modulus 0.02801 GPa
4.063 ksi
ISO 527-2/5A/500
Tear Strength 170 kN/m
970 pli
ISO 34-1B
Abrasion 25
25
loss (mm³); ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 137 °C
279 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 220 °C
428 °F
Zone 1 210 °C
410 °F
Zone 2 215 °C
419 °F
Zone 3 225 °C
437 °F
Zone 4 225 °C
437 °F
Dry Time 3.00 hour

@Temperature 100 °C
3.00 hour

@Temperature 212 °F