Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 40.00 MPa | 5801 psi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T60D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me.. |
|||
Tensile Strength, Yield | 40.00 MPa | 5801 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 11T85UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T85UV is a UV resistant polycaprolactone copolyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, featuring adequate hardness with excellent.. |
|||
Tensile Strength, Yield | 40.00 MPa | 5801 psi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T95P Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T95P is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical p.. |
|||
Tensile Strength, Yield | 40.00 MPa | 5801 psi | ASTM D412 |
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance.. |
|||
Tensile Strength, Yield | 40.00 MPa | 5802 psi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining high hardness with excellent mechanical properties and .. |
|||
Tensile Strength, Yield | 40.00 MPa | 5801 psi | ISO 527-2 |
Borealis Daploy™ WB130HMS High Melt Strength Polypropylene for Foam Extrusion Daploy WB130HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Tensile Strength, Yield | 40.00 MPa | 5801 psi | ISO 527-2 |
Borealis Daploy™ WB135HMS High Melt Strength Polypropylene for Foam Extrusion Daploy WB135HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Tensile Strength, Yield | 40.00 MPa | 5801 psi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T93 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical prop.. |
|||
Tensile Strength, Yield | 40.00 MPa | 5801 psi | At 50 mm/min; ISO 527-2 |
Borealis Bormod™ HF955MO Polypropylene Homopolymer for Injection Molding Bormod HF955MO is a high modulus polypropylene homopolymer. Bormod HF955MO is especially developed within the proprietary Borstar technology. The grade utilizes the unique Borstar reactor design c.. |