Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0150 GPa | 2.18 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T60D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me.. |
|||
50% Modulus | 0.0150 GPa | 2.18 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |