Covestro Desmopan® DP 8377 Polyurethane + ABS

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyurethane Alloy , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 8377 Polyurethane + ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
injection molding grademodified with ABSgood low-temperature flexibilitygood wear resistanceApplicationSki boot shellsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 97
97
3s; ISO 868
Hardness, Shore D 63
63
15s; ISO 868
Abrasion 30
30
mm³; ISO 4649
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America
Feature Release agent
Form Pellets
Process Injection Molding