Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
SABIC PP 578P Polypropylene Homopolymer for Injection Molding Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® DMX3415M PC Copolymer (Europe-Africa-Middle East) Lexan* DMX3415M is a co-polycarbonate resin with improved scratch and abrasion resistance compared to standard polycarbonate. Lexan* DMX3415M is available in transparent colors. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Izod Impact, Notched | 0.300 - 0.500 J/cm @Thickness 3.20 - 3.20 mm |
0.562 - 0.937 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 0.579 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.300 - 7.50 J/cm @Temperature -50.0 - 0.000 °C |
0.562 - 14.1 ft-lb/in @Temperature -58.0 - 32.0 °F |
Average value: 3.76 J/cm Grade Count:89 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATILUB 95-25GR CE/10 Polysulfone Base (PSU), 25% Graphite, 10% Special Mineral Filled Self Lubricating Plastic Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | 23° C; ASTM D256 |
Flint Hills P4C5B-075 Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: tape extrusion and closures.Former Huntsman polypropylene products are now prod.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | 23° C; ASTM D256 |
Flint Hills P4G4B-125A Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Nucleated and antistat.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills .. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | 23° C; ASTM D256 |
Flint Hills P4G4T-017A Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Highly lubricated and antistat.Applications: Injection molding: closures.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Izod Impact, Notched | >= 0.300 J/cm | >= 0.562 ft-lb/in | Method A; ASTM D 256 |
Karina E 800-35/1-Y-CRB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East) VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 815F PBT+PET PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® HX215HP PBT High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta.. |
|||
Izod Impact, Notched | 0.300 - 0.600 J/cm | 0.562 - 1.12 ft-lb/in | ASTM D256 |
Shuman 510 Black Polypropylene Homopolymer Excellent chemical resistance, excellent processabilityData provided by the manufacturer. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.300 J/cm @Thickness 3.17 mm |
0.562 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Washington Penn PPH2UFO Polypropylene, Unfilled Homopolymer for injection molding. Meets General Motors spec. GMP.PP.013Data provided by Washington Penn Plastic Co., Inc. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ISO 180 |
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ISO 180 |
Wellman Wellamid® GS40-66 22L-N 40% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
Total PPH 3576 H Polypropylene Homopolymer, Cast Film Polypropylene 3576 H is recommended for use core layer in non-oriented cast films processes for the manufacture of packaging film with outstanding optical properties. 3576 H is specially designed f.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB901 Nylon 6, Extruded cable coating Polyamide 6 for very thin electrical extruded cable coatingInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-17338 22% CACO3 Filled Copolymer Polypropylene DescriptionPolyfort® E 17338 is a 22% filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 504 XP Bioriented Film Polypropylene Description: H 504XP is a low melt flow rate homopolymer, designed specially for high speed lines of biorented films (BOPP). This product features a broad processing window with high output and regu.. |
|||
Izod Impact, Notched | 0.300 J/cm @Thickness 3.20 mm |
0.562 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® 301-G0 PBT Resin Flame retardant, folding enduranceInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.300 - 0.850 J/cm @Temperature -30.0 - 0.000 °C |
0.562 - 1.59 ft-lb/in @Temperature -22.0 - 32.0 °F |
Average value: 0.547 J/cm Grade Count:13 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.300 - 2.51 J/cm | 0.562 - 4.70 ft-lb/in | Average value: 0.896 J/cm Grade Count:124 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. .. |