Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and draw down ability.Applications: Blend, liners, stretch film.Advantages: Outstanding toughness, high tensile strength and good puncture resistance.Information provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 25.0 microns
0.984 mil
extruded at 2:1 BUR
Base Resin Melt Index 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 450 %
450 %
ASTM D882
Film Elongation at Break, TD 700 %
700 %
ASTM D882
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 13.0 g/micron
330 g/mil
ASTM D1922
Dart Drop 3.00 g/micron
76.2 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
Film Tensile Strength at Break, TD 25.5 MPa
3700 psi
ASTM D882
1% Secant Modulus, MD 166.7 MPa
24180 psi
ASTM D882
1% Secant Modulus, TD 196.14 MPa
28447 psi
ASTM D882
Optical Properties Metric English Comments
Haze 14 %
14 %
ASTM D1003
Gloss 35 %
35 %
45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 160 - 200 °C
320 - 392 °F
Blow-up Ratio (BUR) 2.0 - 3.0
2.0 - 3.0
Users viewing this material also viewed the following: