Polymer Property : Elmendorf Tear Strength, TD = 13.0 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 13.0 g/micron
330 g/mil
ASTM D1922
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin  (discontinued **)
LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and ..
Elmendorf Tear Strength, TD 13.0 g/micron
330 g/mil
ASTM D1922
ExxonMobil ESCOR™ AT 310 Blown Film Resin  (discontinued **)
ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo..
Elmendorf Tear Strength, TD 13.0 g/micron
330 g/mil
ASTM D1922
ExxonMobil Exceed™ 1012CA Film Resin  (discontinued **)
Exceed 1012CA mVLDPE resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1012CA resin have outstanding cold temperature toughness, impact strength a..
Elmendorf Tear Strength, TD 13.0 g/micron
330 g/mil
1 mil; Blown Film; ASTM D1922
Chevron Phillips Marlex® HHM TR-140 Polyethylene, Film Grade; HDPE  (discontinued **)
FDA approved.Data provided by the manufacturer
Elmendorf Tear Strength, TD 13.0 g/micron
330 g/mil
1 mil; Blown Film; ASTM D1922
Chevron Phillips Marlex® HHM TR-144 Polyethylene, Film Grade; HDPE  (discontinued **)
FDA approved.Data provided by the manufacturer
Elmendorf Tear Strength, TD 13.0 g/micron
330 g/mil
ASTM D1922
Reliance Industries Relene F46003 Polyethylene
Relene F46003 is a High Density Polyethylene grade suitable for producing blown parts with superior stiffness and barrier properties. It is recommended for making liners and coextruded film structu..