Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM D882 |
Formosa Plastics Formolene® L62608PE Film (Hexene Grade) LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin
(discontinued **) LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM D882 |
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shri.. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM D882 |
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer Westlake DA591 resin is a 9.0% EVA copolymer designed as a tie layer in multi-layered food packaging film. It has excellent clarity, excellent toughness, good resistance to load deformation, and goo.. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM-D882 |
Westlake Elevate™ EB591 9% EVA Copolymer Westlake EB591 resin is a 9% EVA copolymer designed for films that require excellent toughness and good heat sealing characteristics. This Kosher compliant resin has excellent low temperature brittl.. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM D882 |
Westlake LF1050 Butene Linear Low Density Polyethylene Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr.. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM D882 |
Formosa Plastics Formolene® L62608 Film (Hexene Grade) LLDPE Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM D882 |
ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealabi.. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM D882 |
Dow 751A Low Density Polyethylene Resin A high additive film resin for general packaging applications For cast film extrusion A fast blooming resin for high speed bag conversion Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information p.. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | |
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA) PRIMACOR® 1321 polymer is an EAA copolymer (% comonomer 6.5) for blown and cast films. Its outstanding properties include, excellent sealability, toughness, adhesion and tear resistance. PRIMACOR 1.. |
|||
Film Tensile Strength at Break, MD | 32.4 MPa | 4700 psi | ASTM D882 |
Formosa Plastics Formolene® L62608PA Film (Hexene Grade) LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |