Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
Formosa Plastics Formolene® L62608PE Film (Hexene Grade) LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin  (discontinued **)
LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and ..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade
Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shri..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer
Westlake DA591 resin is a 9.0% EVA copolymer designed as a tie layer in multi-layered food packaging film. It has excellent clarity, excellent toughness, good resistance to load deformation, and goo..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM-D882
Westlake Elevate™ EB591 9% EVA Copolymer
Westlake EB591 resin is a 9% EVA copolymer designed for films that require excellent toughness and good heat sealing characteristics. This Kosher compliant resin has excellent low temperature brittl..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
Westlake LF1050 Butene Linear Low Density Polyethylene
Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
Formosa Plastics Formolene® L62608 Film (Hexene Grade) LLDPE
Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin
Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealabi..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
Dow 751A Low Density Polyethylene Resin
A high additive film resin for general packaging applications For cast film extrusion A fast blooming resin for high speed bag conversion Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information p..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA)
PRIMACOR® 1321 polymer is an EAA copolymer (% comonomer 6.5) for blown and cast films. Its outstanding properties include, excellent sealability, toughness, adhesion and tear resistance. PRIMACOR 1..
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
Formosa Plastics Formolene® L62608PA Film (Hexene Grade) LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he..