Physical Properties Metric English Comments
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin  (discontinued **)
LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANEX® LF1044 Linear low density polyethylene resin  (discontinued **)
LF1044 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down..
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANEX® LF2024 Linear low density polyethylene resin  (discontinued **)
LF2024 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and ..
Base Resin Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin  (discontinued **)
LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and ..
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANEX® LF0754 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF0754 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant agent. This product is used for blown film extrusion which offers outstanding toughness, extrudabilit..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF1054 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and ..
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANEX® LF2554 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF2554 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for slot cast extrusion which offers outstanding toughness, extrudability and d..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin  (discontinued **)
LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance,..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANCEED® mL2764 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL2764 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL2764 have outstanding tensile properties, impact streng..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANCEED® mL3564 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL3564 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL3564 have outstanding tensile properties, impact streng..
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services  (discontinued *
VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t..
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D4883
Eastman 1550F Film Polyethylene  (discontinued **)
Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long..
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D4883
Eastman E6838-902F Polyethylene Film  (discontinued **)
Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business ..
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANLENE® LDI300YY Low density polyethylene resin
LDI300YY is a low density polyethylene resin for injection molding and is a barefoot grade. LDI300YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2..
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANLENE® LDC800YY Low density polyethylene resin
LDC800YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC800YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2..
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin
LDC801YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC801YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2..
Copyright © lookpolymers.com All Rights Reserved