Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin Film Properties. Features: Free flowing granules, toughness and strength, ease of extrusion.Applications: Blending, concentrates.Data provided by the manufacturer. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, bags-on-roll, garment film.Data provided by the manufacturer. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F<sub>50</sub>,38mm dart 66mm height; ASTM D1709 |
Reliance Industries Reclair F22020 Polyethylene Butene comonomer based Linear Low Density Polyethylene blow film grade. Reclair F22020 has optimum levels of antioxidants, antiblocking agents, and slip additives. Applications:general purpose, and.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealing characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | ASTM D1709 |
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin
(discontinued **) LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Novapol® LF-Y819-C LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F<sub>50</sub>, ASTM D1709/A |
NOVA Chemicals Novapol® PF-0218-F Butene LLDPE Film Resin Toughness and strength, Ease of extrusionApplications: Cast films, BlendingAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depende.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, general purpose packaging, garment film.Data provided by the manufacturer. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F<sub>50</sub>,38mm dart 66mm height; ASTM D1709 |
Reliance Industries Reclair F18020 Polyethylene Butene comonomer based Linear Low Density Polyethylene cast film grade. Reclair F18020 has optimum levels of antioxidants, and polymer processing aids. Applications:cast films, air bubble films, an.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Sclair® 14A Butene MDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness, broad MW distribution.Applications: Co-extrusion, blending.Data provided by the manufacturer. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F50; ISO 7765-A |
Carmel Olefins IPETHENE® 214 Low Density Polyethylene
(discontinued **) IPETHENE® 214 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. APPLICATIONS IPETHENE® 214 is main.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | ASTM D1709 |
Lotte Chemical Titan TITANLENE® LDF264YZ Low density polyethylene LDF264YZ is a low density polyethylene resin for film extrusion. LDF264YZ has no slip and anti-block additives. LDF264YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | |
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | |
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F50; ISO 7765-A |
Carmel Olefins IPETHENE® 210 Low Density Polyethylene IPETHENE® 210 is a low density polyethylene extrusion grade, containing no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 210 is mainly u.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F50; ISO 7765-A |
Carmel Olefins IPETHENE® 213 Low Density Polyethylene IPETHENE® 213 is a general purpose low density polyethylene film extrusion grade. It contains a medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between .. |
|||
Dart Drop | 3.00 - 19.7 g/micron | 76.2 - 500 g/mil | Average value: 6.47 g/micron Grade Count:12 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | ASTM D1709A |
Eastman E6838-975F Polyethylene
(discontinued **) E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film.. |
|||
Dart Drop | 3.00 g/micron | 76.2 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Sclair® 14J1 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, high strength and toughness.Applications: Produce film.Data provided by the manufacturer. |