Material Notes:
Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regulation Title CFR, Paragraph 175.300.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
9947B; ASTM D1475-85
1.00 g/cc
0.0361 lb/in³
Mixed; ASTM D1475-85
1.10 g/cc
0.0397 lb/in³
9947A; ASTM D1475-85
Solids Content 0.82 %
0.82 %
9947B; by volume; ASTM D2369-87 Modified
1.64 %
1.64 %
9947B; by weight; ASTM D2369-87 Modified
12 %
12 %
Mixed; by volume; ASTM D2369-87 Modified
22 %
22 %
Mixed; by weight; ASTM D2369-87 Modified
22.4 %
22.4 %
9947A; by volume; ASTM D2369-87 Modified
34 %
34 %
9947A; by weight; ASTM D2369-87 Modified
Volatile Organic Compounds (VOC) Content 682 g/l
682 g/l
9947A; ASTM D3960-87
815 g/l
815 g/l
Mixed; ASTM D3960-87
926 g/l
926 g/l
9947B; ASTM D3960-87
Brookfield Viscosity 400 cP
400 cP
ASTM D2196-66; LVT, Spindle #2 @ 30rpm
3000 cP
3000 cP
ASTM D2196-66; LVT, Spindle #2 @ 30rpm
10 cP

@Temperature 25.0 °C
10 cP

@Temperature 77.0 °F
ASTM D2196-66; LVT, Spindle #1 @ 60rpm
Viscosity Measurement 58 - 62
58 - 62
seconds; Zahn, #4 cup
166 - 170
166 - 170
seconds; Zahn, #2 cup
Mechanical Properties Metric English Comments
Impact Test 18.1 J
13.3 ft-lb
Direct; Gardner
18.1 J
13.3 ft-lb
Reverse; Gardner
Thermal Properties Metric English Comments
Flash Point 19.0 °C
66.2 °F
9947B; Setaflash, Closed Cup; ASTM D3278-82
21.0 °C
69.8 °F
9947A; Setaflash, Closed Cup; ASTM D3278-82
Processing Properties Metric English Comments
Dry Time 0.33 hour

@Temperature 22.2 °C
0.33 hour

@Temperature 72.0 °F
Set to touch; Gardner, Mechanical
1.5 hour

@Temperature 22.2 °C
1.5 hour

@Temperature 72.0 °F
Surface Dry; Gardner, Mechanical
2 hour

@Temperature 22.2 °C
2 hour

@Temperature 72.0 °F
Dry Hard; Gardner, Mechanical
Pot Life 120 - 180 min
120 - 180 min
Ready for topcoating
Shelf Life 12.0 Month
12.0 Month
9947B
6.00 Month

@Temperature <=27.0 °C
6.00 Month

@Temperature <=80.6 °F
9947A
Descriptive Properties Value Comments
Appearance Clear, colorless to straw
9947B
Red
Mixed
Red
9947A
Coating Film Dry Weight (gm/ft²/mil) 4.41
Conical Mandrel Bend Passes 1/8"
ASTM D522
Mix Ratio 1:1
by volume
8.9:7.9
by weight
Users viewing this material also viewed the following: