Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brookfield Viscosity = 3000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 3000 - 8000 cP
3000 - 8000 cP
DOP 60phr, 6RPM; ASTM D1824-90
LG Chemical LP170 PVC
General Description: LP170, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170 can be used for sy..
Brookfield Viscosity 3000 - 4000 cP
3000 - 4000 cP
DOP 60phr, 6RPM; ASTM D1824-90
LG Chemical LP170G PVC
General Description: LP170G, homopolymer made from micro- suspension polymerization, is a low viscosity PVC resin with an good deaeration and stable viscosity at high temperature. Products made from..
Brookfield Viscosity 3000 cP
3000 cP
9924A; ASTM D2196-66; LVT, Spindle #3 @ 12rpm
Lord Adhesives Aeroglaze® 9924 Wash Primer
Aeroglaze® 9924 wash primer was designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.All information provided by ..
Brookfield Viscosity 3000 cP
3000 cP
9924A; ASTM D2196-66; LVT, Spindle #3 @ 12rpm
Lord Adhesives Aeroglaze® 9924V Wash Primer
Aeroglaze® 9924V wash primer was designed for priming metal surfaces. It is particularly useful for priming non-ferrous substrates such as aluminum and galvanized steel.All information provided b..
Brookfield Viscosity 3000 cP
3000 cP
ASTM D2196-66; LVT, Spindle #2 @ 30rpm
Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free
Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul..
Brookfield Viscosity 3000 - 22500 cP
3000 - 22500 cP
Fusor 2001; LVT, Spindle #4 @ 30rpm
Lord Adhesives Fusor® 2001 / 2002 Urethane Adhesive
Fusor® 2001/2002 is a two-part urethane adhesive system used to bond fiberglass reinforced plastics, sheet molded compound, and bulk molded compound to themselves as well as to primed metals.All ..
Brookfield Viscosity 3000 - 5000 cP
3000 - 5000 cP
Measured on 25% mass solution in toluene at 25°C; KM 06
Kraton® D1101 B (SBS) Liner Block Copolymer
Description: Kraton D1101 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from South America in the physical form(s) identifi..
Brookfield Viscosity 3000 cP

@Temperature 23.0 °C
3000 cP

@Temperature 73.4 °F
20% T.S. in MEK; 20 RPM; RVT Spindle #2
Lubrizol Estane® 5712 Thermoplastic Polyurethane
Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl..
Brookfield Viscosity 3000 - 5000 cP

@Temperature 191 °C
3000 - 5000 cP

@Temperature 375 °F
3M Scotch-Weld™ 6111 Green Bulk only Adhesive
Same as 6111 tan but green in colorInformation provided by 3M
Brookfield Viscosity 3000 cP
3000 cP
Thermosel using spindle #27
3M Scotch-Weld™ EZ250120 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w..
Brookfield Viscosity 3000 cP
3000 cP
Thermosel using spindle #27
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Brookfield Viscosity 3000 cP
3000 cP
Part A; ASTM D2393
BCC Products DP-11-88 Urethane Adhesive
DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions ..
Brookfield Viscosity 3000 - 5000 cP

@Temperature 191 °C
3000 - 5000 cP

@Temperature 375 °F
3M Scotch-Weld™ 6111 Tan Bulk only Adhesive
Sprayable 100% solventless adhesive for most foams, fabrics, plastics, particle board and thin metalInformation provided by 3M
Brookfield Viscosity 3000 cP
3000 cP
BCC Products BC 8675E Polyurethane Elastomer
BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f..
Copyright © lookpolymers.com All Rights Reserved