Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 1.5 hour @Temperature 22.2 °C |
1.5 hour @Temperature 72.0 °F |
Surface Dry; Gardner, Mechanical |
Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul.. |