Processing Properties Metric English Comments
Pot Life 9.00 - 180 min
9.00 - 180 min
Average value: 64.2 min Grade Count:28
Overview of materials for Epoxy Adhesive, Flexible
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro..
Pot Life 120 - 180 min

@Temperature 20.0 °C
120 - 180 min

@Temperature 68.0 °F
Permabond ET538 Epoxy Resin
PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia..
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
100 gm mass
Resin Technology Group TIGA 159 LV-UV Low Viscosity, Quick Gel UV Initiated, Flexible Epoxy Adhesive
Mix ratio 2 to 1 by volume.TIGA 159 LV-UV hybrid epoxy system is a low viscosity adhesive designed for small potting applications, bonding, laminating, sealing and structural repair applications whe..
Pot Life 120 - 180 min
120 - 180 min
Ready for topcoating
Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free
Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul..
Pot Life 120 - 180 min

@Temperature 23.9 °C
120 - 180 min

@Temperature 75.0 °F
Devcon Tile Adhesive Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Pot Life 120 - 180 min
120 - 180 min
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy
Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr..
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
100 g
Armstrong A-4/E Epoxy Adhesive
Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe..
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
100 g
Armstrong A-5/E Epoxy Adhesive
Information provided by Ellsworth Adhesives.
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
100 g
Armstrong C-1/E Epoxy Adhesive
A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor..
Pot Life 120 - 180 min

@Temperature 24.0 °C
120 - 180 min

@Temperature 75.2 °F
BCC Products BC 7020 Epoxy Backfill System
BC 7020 is a lightweight two component epoxy backfill system. Unlike BC 7010, the filler portion is pre-blended into the resin and hardener components for easier handling, thus simplifying the mixin..
Pot Life 120 - 180 min
120 - 180 min
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina
Coarse grain castable for producing large hi-temp tooling.
Pot Life 120 - 180 min
120 - 180 min
Abatron AboCast 22-30/AboCure 50-4 Epoxy
AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A..
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
100 g
Armstrong A-1/E Epoxy Adhesive
A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El..
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
100 g
Armstrong A-3/E Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..
Pot Life 120 - 180 min
120 - 180 min
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound
Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils ..
Pot Life 120 - 180 min
120 - 180 min
Abatron AboCast 50-11/AboCure 50-4 Epoxy
AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A..
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
1-2 lbs
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge cas..
Copyright © lookpolymers.com All Rights Reserved