Material Notes:
Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an impetus powder with white colorOverview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a wide variety of application. Common examples of polycarbonate products include electronic and electrical component vehicles, CD/DVD and food and drink containers. In addition, epoxy resins are most commonly used as protective coatings, and adhesives. BPA is produced through a catalyzed condensation reaction of phenol with acetone. CAS: 287-92-3Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Bulk Density 0.630 - 0.680 g/cc
0.0228 - 0.0246 lb/in³
Molecular Weight 228.3 g/mol
228.3 g/mol
Vapor Pressure 0.000267 bar

@Temperature 170 °C
0.200 torr

@Temperature 338 °F
Thermal Properties Metric English Comments
Heat of Fusion 125 J/g
53.8 BTU/lb
Specific Heat Capacity 1.51 J/g-°C

@Temperature 60.0 °C
0.361 BTU/lb-°F

@Temperature 140 °F
1.88 J/g-°C

@Temperature 157 °C
0.449 BTU/lb-°F

@Temperature 315 °F
solid
2.34 J/g-°C

@Temperature 165 °C
0.559 BTU/lb-°F

@Temperature 329 °F
2.55 J/g-°C

@Temperature 157 °C
0.609 BTU/lb-°F

@Temperature 315 °F
liquid
Melting Point >= 156.5 °C
>= 313.7 °F
Freezing Point
157 °C
315 °F
Boiling Point 360.5 °C
680.9 °F
Flash Point 207 °C
405 °F
COC
227 °C
441 °F
CC
Electrical Properties Metric English Comments
Volume Resistivity 5.10e+15 ohm-cm
5.10e+15 ohm-cm
Descriptive Properties Value Comments
Color <10 APHA
Solution color
<20 APHA
Molten color
White prills
Explosion limit 0.019 g/l
Ignition Point 532°C
Purity >99.85T