Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.630 - 0.680 g/cc | 0.0228 - 0.0246 lb/in³ | |
LG Chemical BPA Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an us powder with white colorOverview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a w.. |