Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 157 °C | 315 °F | Flow temperature; ASTM D569 |
Plaskolite Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Melting Point | 157 °C | 315 °F | Flow Temperature; ASTM D569 |
Plaskolite PL-24 Acrylic Resin For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer. |
|||
Melting Point | 157 °C | 315 °F | Flow temperature; ASTM D569 |
Plaskolite West Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line. |
|||
Melting Point | 157 °C | 315 °F | Flow temperature; ASTM D569 |
Plaskolite Optix® PL-30 Acrylic Resin
(discontinued **) Injection molding and extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line with exceptional mold release.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Melting Point | 157 °C | 315 °F | Flow temperature; ASTM D569 |
Plaskolite Optix® PL-52 Acrylic Resin
(discontinued **) Injection/extrusion pellets. High heat resistance/medium flow.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Melting Point | 157 °C | 315 °F | |
LG Chemical BPA Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an us powder with white colorOverview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a w.. |
|||
Melting Point | 157 °C | 315 °F | |
Indium Corp. 4N Commercial Indium Metal Indium is a versatile metal with unique physical properties.Indium has one of the widest liquid temperature ranges of any metal.Indium has a low vapor pressure, making it ideal for high vacuum appli.. |
|||
Melting Point | 157 °C | 315 °F | |
Indium Corp. 5N Commercial Indium Metal Indium is a versatile metal with unique physical properties.Indium has one of the widest liquid temperature ranges of any metal.Indium has a low vapor pressure, making it ideal for high vacuum appli.. |
|||
Melting Point | 157 °C | 315 °F | |
Indium Corp. Indalloy® 4 Pure Indium Solder Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni.. |
|||
Melting Point | 157 °C | 315 °F | ASTM D4591 |
Westlake Plastics Kynar® 2850 PVDF Copolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Melting Point | 157 °C | 315 °F | |
Williams Advanced Alloys WS157 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 157 °C | 315 °F | DSC |
Total PPH 3847MR Polypropylene, Radiation Resistant - Clarified - High Flow for Injection Molding TOTAL Petrochemicals Polypropylene 3847MR offers good processability, excellent clarity, good toughness and good resistance to typical levels of gamma radiation used to sterilize polypropylene.Easy .. |
|||
Melting Point | <= 157 °C | <= 315 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 7741 Ethylene Vinyl Acetate Copolymer Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends.. |
|||
Melting Point | 157 °C | 315 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Melting Point | 157 °C | 315 °F | |
Indium Corp. 3N Commercial Indium Metal Indium is a versatile metal with unique physical properties.Indium has one of the widest liquid temperature ranges of any metal.Indium has a low vapor pressure, making it ideal for high vacuum appli.. |