Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 360.5 °C | 680.9 °F | |
LG Chemical BPA Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an us powder with white colorOverview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a w.. |