Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Boiling Point = 680.9 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 360.5 °C
680.9 °F
LG Chemical BPA
Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an us powder with white colorOverview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a w..
Copyright © lookpolymers.com All Rights Reserved