Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 31.7 MPa | 4590 psi | |
Ohio Carbon Blank OCB EDM-200 Mechanical Grade Graphite Available in a range of sizes and shapes. |
|||
Tensile Strength | 31.7 MPa | 4600 psi | ASTM D638 |
Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet) Natural and Black |
|||
Tensile Strength | 31.7 MPa | 4600 psi | ASTM D638 |
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |
|||
Tensile Strength | 31.7 MPa | 4600 psi | measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D1101 K (SBS) Liner Block Copolymer Kraton D1101 K is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified:Kraton D1101 .. |
|||
Tensile Strength | 31.7 MPa | 4600 psi | measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D1102 K (SBS) Liner Block Copolymer Description: Kraton D1102 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 28%. It is supplied from North America in the physical form identified.. |
|||
Tensile Strength | 31.7 MPa | 4600 psi | Typical properties on film cast from toluene solution; ASTM D412 |
Kraton® D1114 P (SIS) Linear Triblock Copolymer Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: .. |
|||
Tensile Strength | 31.7 MPa | 4600 psi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® D1116 K (SBS) Radial Triblock Copolymer Description: Kraton D1116 K is a clear, radial triblock copolymer based on styrene and butadiene, with a polystyrene content of 23%. It is supplied from North America in the physical form identified.. |
|||
Tensile Strength | 31.7 MPa | 4600 psi | ASTM D638 |
Ecomass® 1080CO94 Copper Powder Filled Polyamide Alloy, Injection Molding Moderate Specific Gravity, Copper Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing.. |
|||
Tensile Strength | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
Braskem TI2150C High Crystallinity Copolymer Polypropylene Description: Highly crystalline homopolymer phase, very high molecular weight ERP phase, very high flexural Modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding... |
|||
Tensile Strength | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
Braskem TI2350C High Crystallinity Copolymer Polypropylene Description: Highly crystalline homopolymer phase, very high molecular weight ERP phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding... |
|||
Tensile Strength | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
Braskem TI4150WR Impact Copolymer Polypropylene Description: Very good mold release, very high flexural modulus.Applications: Suggested uses include closures, housewares.Process: Injection Molding.This resin meets the requirements for olefin poly.. |
|||
Tensile Strength | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
Braskem TR3020C Random Copolymer Polypropylene Description: Clarified, high flexural modulus. Applications: Suggested uses include extrusion, blow molding, thermoforming. Process: Blow Molding. This resin meets the requirements for olefin polym.. |
|||
Tensile Strength | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
Braskem TR3020NT Random Copolymer Polypropylene Description: High flexural modulus, very good mold release. Applications: Suggested uses include extrusion, compression molding, thermoforming. Process: Compression Molding. This resin meets the req.. |
|||
Tensile Strength | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
Braskem TR3350UC Random Copolymer Polypropylene Description: Maximum see-through clarity, minimal haze; superior color stability, process stability, and gloss; low odor, high melt flow.Applications: Suggested uses; reusable food containers, house.. |