Polymer Property : Bulk Density = 0.449 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.449 g/cc
0.0162 lb/in³
Kraton® D1102 K (SBS) Liner Block Copolymer
Description: Kraton D1102 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 28%. It is supplied from North America in the physical form identified..
Bulk Density 0.449 - 0.497 g/cc
0.0162 - 0.0179 lb/in³
Loose
KaMin KaMin® 35 Kaolin Clay - Waterwashed
Coarse kaolin, milled powder, with the lowest oil absorption, for extending without thickening.Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Wood..
Bulk Density 0.449 g/cc
0.0162 lb/in³
As Supplied
Skamol Group Moler 10 Aggregate Insulation
SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre..
Bulk Density 0.449 g/cc
0.0162 lb/in³
DayGlo Gem-Tone GC-19F Sapphire Blue
Gem-Tone™ Sapphire Blue is a rich blue colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of this colorant. N..
Bulk Density 0.449 g/cc
0.0162 lb/in³
Loose
CIMBAR CIMTUFF® 9110 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..
Bulk Density 0.449 g/cc
0.0162 lb/in³
Loose
CIMBAR MV 610 Talc
MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla..
Bulk Density 0.449 - 0.497 g/cc
0.0162 - 0.0179 lb/in³
Loose
KaMin Polyfil® 35 Kaolin Clay - Waterwashed
Coarse kaolin, with the lowest oil absorption, for extending without reinforcement, milled powder form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, General Plastics, SMC/B..