Mechanical Properties Metric English Comments
Tensile Strength 31.7 MPa
4600 psi
ASTM D638
Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet)
Natural and Black
Tensile Strength 31.7 MPa
4600 psi
ASTM D638
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet)
Tensile Strength 31.7 MPa
4600 psi
measured on films cast from a solution in toluene; ASTM D412
Kraton® D1101 K (SBS) Liner Block Copolymer
Kraton D1101 K is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified:Kraton D1101 ..
Tensile Strength 31.7 MPa
4600 psi
measured on films cast from a solution in toluene; ASTM D412
Kraton® D1102 K (SBS) Liner Block Copolymer
Description: Kraton D1102 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 28%. It is supplied from North America in the physical form identified..
Tensile Strength 31.7 MPa
4600 psi
Typical properties on film cast from toluene solution; ASTM D412
Kraton® D1114 P (SIS) Linear Triblock Copolymer
Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: ..
Tensile Strength 31.7 MPa
4600 psi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® D1116 K (SBS) Radial Triblock Copolymer
Description: Kraton D1116 K is a clear, radial triblock copolymer based on styrene and butadiene, with a polystyrene content of 23%. It is supplied from North America in the physical form identified..
Tensile Strength 31.7 MPa
4600 psi
ASTM D638
Ecomass® 1080CO94 Copper Powder Filled Polyamide Alloy, Injection Molding
Moderate Specific Gravity, Copper Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing..
Tensile Strength 31.7 MPa
4600 psi
2 in/min; ASTM D638
Braskem TI2150C High Crystallinity Copolymer Polypropylene
Description: Highly crystalline homopolymer phase, very high molecular weight ERP phase, very high flexural Modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding...
Tensile Strength 31.7 MPa
4600 psi
2 in/min; ASTM D638
Braskem TI2350C High Crystallinity Copolymer Polypropylene
Description: Highly crystalline homopolymer phase, very high molecular weight ERP phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding...
Tensile Strength 31.7 MPa
4600 psi
2 in/min; ASTM D638
Braskem TI4150WR Impact Copolymer Polypropylene
Description: Very good mold release, very high flexural modulus.Applications: Suggested uses include closures, housewares.Process: Injection Molding.This resin meets the requirements for olefin poly..
Tensile Strength 31.7 MPa
4600 psi
2 in/min; ASTM D638
Braskem TR3020C Random Copolymer Polypropylene
Description: Clarified, high flexural modulus. Applications: Suggested uses include extrusion, blow molding, thermoforming. Process: Blow Molding. This resin meets the requirements for olefin polym..
Tensile Strength 31.7 MPa
4600 psi
2 in/min; ASTM D638
Braskem TR3020NT Random Copolymer Polypropylene
Description: High flexural modulus, very good mold release. Applications: Suggested uses include extrusion, compression molding, thermoforming. Process: Compression Molding. This resin meets the req..
Tensile Strength 31.7 MPa
4600 psi
2 in/min; ASTM D638
Braskem TR3350UC Random Copolymer Polypropylene
Description: Maximum see-through clarity, minimal haze; superior color stability, process stability, and gloss; low odor, high melt flow.Applications: Suggested uses; reusable food containers, house..