Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 73.3 °C | 164 °F | ASTM D-648 |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.4 °C @Thickness 3.18 mm |
164 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 86110 white 1275 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.3 °C @Thickness 3.18 mm |
164 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700X Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.3 °C | 164 °F | ASTM D-648 |
Plaskolite Optix® CP - 927 GHF High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.3 °C @Thickness 3.18 mm |
164 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L4536 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.3 °C | 164 °F | ASTM D-648 |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.3 °C | 164 °F | ASTM D648 |
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.3 °C | 164 °F | unannealed; ASTM D648 |
KYDEX® 430 ABS/PVC Blend for Medical Device Housings KYDEX® 430 is an ABS/PVC thermoplastic sheet that offers superior thermoformability, rigidity, breakage resistance, chemical resistance and fire retardancy.Features:Good for deep or hard to form .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.3 °C | 164 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® NN300TL (Dry) Nylon 66, Lubricated, Impact Modified, Recycled Content Features: Impact modifiedGood toughnessLubricatedRecycled ContentForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.3 °C | 164 °F | ASTM D-648 |
Plaskolite West Optix® CP - 927 GHF High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |