Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KKPC Kuhmo GP 125H High Transparency GPPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Transparent Grade
Manufacturer Korea Kumho Petrochemical Co., Ltd.
Trade Name Kuhmo
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KKPC Kuhmo GP 125H High Transparency GPPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key features: High Transparency Common Uses: Humidifiers, optical instruments.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability of dimension.Data provided by Korea Kumho Petrochemical Co., Ltd.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 1.5 g/10 min
1.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
ASTM D785
Tensile Strength, Ultimate 49.9 MPa
7240 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 89.273 MPa
12948 psi
ASTM D790
Flexural Modulus 2.888 GPa
418.9 ksi
ASTM D790
Izod Impact, Notched 0.149 J/cm

@Thickness 3.20 mm
0.280 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
189 °F
unannealed; ASTM D648
Vicat Softening Point 105 °C
221 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 2.20 mm
HB

@Thickness 0.0866 in
HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr species transparent but does not quantify
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 21.7 kV/mm
550 kV/in
ASTM D149
Users viewing this material also viewed the following: