Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 89.273 MPa | 12948 psi | ASTM D790 |
KKPC Kuhmo GP 125H High Transparency GPPS Key features: High Transparency Common Uses: Humidifiers, optical instruments.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability.. |