KEP Kepital® TX-31 Wear/Friction/Resistant Acetal Copolymer

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer Korea Engineering Plastics Co., Ltd.
Trade Name Kepital®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KEP Kepital® TX-31 Wear/Friction/Resistant Acetal Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Kepital® is a registered trademark of Korea Engineering Plastics Co., Ltd. Information provided by Dayson Polymers.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ASTM D955
Melt Flow 27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 53.93 MPa
7822 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Yield Strength 79.43 MPa
11520 psi
ASTM D790
Flexural Modulus 2.44 GPa
354 ksi
ASTM D790
Izod Impact, Notched 0.737 J/cm
1.38 ft-lb/in
ASTM D256
Coefficient of Friction 0.10
0.10
Polymer to Polymer; KEP Method
0.10
0.10
Polymer to Steel; KEP Method
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 156.0 °C
312.8 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107.0 °C
224.6 °F
ASTM D648
Flammability, UL94 HB