Tensile Strength at Break | 53.93 MPa | 7822 psi | ASTM D638 |
KEP Kepital® TX-31 Wear/Friction/Resistant Acetal Copolymer Kepital® is a registered trademark of Korea Engineering Plastics Co., Ltd. Information provided by Dayson Polymers. |