LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: medium high melt flow, medium high modulus, flame retardant, low specific gravity, good impact strengthApplications: battery jars, electrical componentsDescription: Astryn BA905-74 medium high melt flow, UL 94 V-0 flame retardant polypropylene copolymer has a very good combination of properties and processability. It was designed for applications which have stringent flammability requirements.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792B
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
Tool, Montell
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 225 %
225 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256A
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 30 %
30 %
ASTM D2863