Mechanical Properties Metric English Comments
Flexural Modulus 2.44 GPa
354 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according ..
Flexural Modulus 2.44 GPa
354 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS
Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior...
Flexural Modulus 2.44 GPa
354 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior...
Flexural Modulus 2.44 GPa
354 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications
Flexural Modulus 2.44 GPa
354 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP ..
Flexural Modulus 2.44 GPa
354 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Flexural Modulus 2.44 GPa
354 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Flexural Modulus 2.44 GPa
354 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP COLORCOMP D10006U PC
LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed.
Flexural Modulus 2.44 GPa
354 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Asia Pacific)
Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior...
Flexural Modulus 2.44 GPa
354 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific)
CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications
Flexural Modulus 2.44 GPa
354 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Flexural Modulus 2.44 GPa
354 ksi
ASTM D790
KEP Kepital® TX-31 Wear/Friction/Resistant Acetal Copolymer
Kepital® is a registered trademark of Korea Engineering Plastics Co., Ltd. Information provided by Dayson Polymers.
Flexural Modulus 2.44 GPa
354 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS
LNP LUBRICOMP* NL001 is a compound b ased on PC+ABS resin containing 5% PTFE. Added features include: Wear Resistant, Suitable for Thin Wall Applications.
Flexural Modulus 2.44 GPa
354 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS (Europe-Africa-Middle East)
LNP LUBRICOMP* NL001 is a wear resistant PC+ABS blend, suitable for thin wall applications.
Flexural Modulus 2.44 GPa
354 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL PX1391 PPE+PS
PPE+PS blend. Unfilled. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Flexural Modulus 2.44 GPa
354 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL PX1391 PPE+PS (Asia Pacific)
Automotive applications, primarily. Excellent electrical properties. high heat. 305F (152C) DTUL.
Flexural Modulus 2.44 GPa
354 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 243 Ionomer
Information provided by A. Schulman.
Flexural Modulus 2.44 GPa
354 ksi
ISO 178
Polyplastics Duranex® 200FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Flow
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 2.44 GPa
354 ksi
ISO 178
Polyplastics Duranex® 300FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Flow
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 2.44 GPa
354 ksi
ISO 178
Polyplastics Duranex® 500FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 2.44 GPa
354 ksi
ISO 178
Polyplastics Duranex® 800FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Viscosity
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 2.44 GPa
354 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 243 Ionomer
Information provided by A. Schulman.
Flexural Modulus 2.44 GPa
354 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 243 Ionomer
Information provided by A. Schulman.
Flexural Modulus 2.44 GPa
354 ksi
ISO 178
Polyplastics Duranex® 700FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Viscosity
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 2.44 GPa
354 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 243 Ionomer
Information provided by A. Schulman.
Flexural Modulus 2.44 GPa
354 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 243 Ionomer
Information provided by A. Schulman.
Flexural Modulus 2.44 GPa
354 ksi
ASTM D790
Eastman Eastar EN010 Copolyester
Eastar copolyester EN010 is used primarily in molded thick wall European applications.Applications/UsesPackagingInjection moldingContainers
Flexural Modulus 2.44 GPa
354 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 243 Ionomer
Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved