Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 107.0 °C | 224.6 °F | ASTM D648 |
KEP Kepital® TX-31 Wear/Friction/Resistant Acetal Copolymer Kepital® is a registered trademark of Korea Engineering Plastics Co., Ltd. Information provided by Dayson Polymers. |