Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 27 g/10 min | 27 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite Optix® CA-41 General Purpose Acrylic Resin Injection Molding Grade Pellets only. Lowest Heat Resistance and maximum flow. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MS 80 U High Density Polyethylene - Injection Molding Eraclene MS 80 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This grade has a narrow molecular weight distribution and a hig.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 210 °C |
27 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
NatureWorks® Ingeo™ AW 300D Injection Grade Biopolymer Specifically designed for use in injection molded food serviceware applications. This opaque, off-white molding grade creates parts that are rigid and heat resistant for tableware used with hot food.. |
|||
Melt Flow | 27 g/10 min @Load 1.20 kg, Temperature 300 °C |
27 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 905AU PC (Asia Pacific) LEXAN resin grade 905AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in all colors, intended to .. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MS 80 High Density Polyethylene - Injection Molding Eraclene MS 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MS 80 shows a good balance between processability and mechanical pro.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
PolyOne Edgetek® 5230 Natural 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Melt Flow | 27 - 37 g/10 min @Load 10.0 kg, Temperature 420 °C |
27 - 37 g/10 min @Load 22.0 lb, Temperature 788 °F |
ASTM D1238 |
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
27 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Pro-fax PF531 Polypropylene Homopolymer, Radiation Resistant Primary Processing Method: Injection MoldingKey Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation st.. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Flint Hills P5M6K-080 Polypropylene Random Copolymer Features: Clarified, Gamma Radiation Sterilizable. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: Disposable Syringes. This product is not rec.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 240 °C |
27 g/10 min @Load 4.76 lb, Temperature 464 °F |
ASTM D1238 |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | |
Intercontinental Polymers 554 PBT Polymer Type - Elastomer Polyester Pellets Applications: Engineering Resin - ModifiedInformation provided by Intercontinental Polymers. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 260 °C |
27 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6, 40% Glass Fiber + Mineral PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 250 °C |
27 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1023P PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 220 °C |
27 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 250 °C |
27 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1023P PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 300 °C |
27 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL ZM3242 PPE+PS (Asia Pacific) Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degC |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 240 °C |
27 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Cossa Polimeri ESTABLEND PA 3000 ABS / Nylon 6 Blend ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri.. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 240 °C |
27 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Cossa Polimeri ESTABLEND PA 2516 GF ABS / Nylon 6 Blend, 8% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedExceptional chemical resistance, excellent heat resistance, good dimensional stabilityInformation .. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 220 °C |
27 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE) ASPUN™ 6811A Fiber Grade Resin: Suggested Optimum Process: Spun Bond Typical Application: Non-woven FabricsInformation provided by Dow |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Aclo Accucomp Polyacetal (POM) ACE093L Low Viscosity |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 500 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
PTS POM-270 Acetal Copolymer Information provided by PTS LLC. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polyram RamTal PM1027 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |